Silver micas as coupling caps?

Status
Not open for further replies.
Hi,

Since they come pretty close to being the "ideal capacitor", they should be fine

Amen to that...
350VDC is likely to be a little low for some applications so be careful where you put them.

I'm curious to know what you think about the sound, never found them in .100µF values.
Mostly use them in RIAA correction where they do an excellent job.

Cheers,😉
 
Hi Peter,

Thanks.
Interesting thread...
To be perfectly honest, I had no idea whatsoever those small values even existed in Teflon.

Currently I use polysterenes or metalized polypropylenes for the simple reason that I don't easily find the silvered micas in the values and tolerances I need.

Metallic powder,he? Never noticed any of it, I swear.
Then again it's not that obvious when you use only a pair per channel burried in a correction network, I presume.

Next time I'll give the Teflons I fair shot.

Cheers,😉

P.S. I had no idea one could catch a handful of philosophers just by posting an excerpt of a book...

SLIPPERY SLOPES.... 😉
 
Hi there,

Honestly speaking, I had got an all FET preamp using silver mica capacitor on the feedback channel. This silver mica capacitor is from RS components and have a tolerance of 0.5%

What I should say the sound will be a little bit metallic on the high frequency range. After that I changed the cap into a pp one. The outcome is more musical and natural.

I recommend the application for silver mica cap should be in precision instrument NOT audio.

Rgds,
Red:smash:
 
A couple of CRC Teflcon caps the small one is a .0012 and the larger one is a 1uf @100 volts. these are great caps for audio.
 

Attachments

  • teflon crc caps2.jpg
    teflon crc caps2.jpg
    91 KB · Views: 555
Hi,

When I checked out CRC's website last night I noticed the small values we often need for RIAA correction networks in valve circuits aren't available in PTFE anyway.

By small I mean the range from say, 100pF to 47nF @ 400VDC.

So in most cases it's either silvered mica or polystyrenes (being fased out) or the new polypropylenes.

On paper at least the micas are closer to the ideal cap than any of the other types.

Cheers,😉
 
Status